Tasirin Cellulose Erther HPMC a kan aikin turmi na kai

Matsakaicin kai na kai na iya dogaro da nauyinsa na kanshi don samar da gidaje mai laushi don samar da manyan kayan, kuma a lokaci guda zai iya aiwatar da manyan abubuwa da ingantacciyar gini. Saboda haka, high mai ruwa mai mahimmanci shine babban al'amari na turmi na kai kai. Bugu da kari, dole ne ya riƙe wani riƙewar ruwa da ƙarfi, babu wani sabon abu na ruwa, kuma suna da halayen rufin zafi da ƙarancin zafin jiki.

Gabaɗaya, turmi na kai yana buƙatar kyakkyawan ruwan rai, amma ruwan sanyi na ainihi shine kawai 10-300px; Elerlulose ether shine babban adadin turmi-hade, kodayake yana da ƙari haɓaka aikin tury, yana iya inganta daidaiton turmi, aikin aiki da kuma amfani da ruwa mai riƙe da ruwa na turmi. Yana taka muhimmiyar rawa a fagen shirye-shiryen turbuwa.

1. Abin farin ciki: eth ether yana da tasiri mai mahimmanci akan riƙe ruwa, daidaito da aikin ginin haɓaka kai na kai. Musamman a matsayin turmi na kai na kai, mai ruwa shine ɗayan manyan alamu don kimanta aikin matakin kai. A karkashin tsarin tabbatar da tsarin turmi na al'ada na turmi, da ruwa mai ruwa ana iya daidaita ta ta hanyar canza adadin sel selulose. Koyaya, idan adadin ya yi yawa, ruwan zãfi zai ragu, don haka adadin sel ether hpmc ya kamata a sarrafa shi cikin kewayon da ya dace.

2. Rarraba Ruwa: Raurin Raudewa na turmi muhimmancin nuna alama ne don auna kwanciyar hankali ta kayan haɗin ciki na tursasced ciminti turgi. Don cikakken aiwatar da hydration dauki na gel kayan, wani adadin selulose eth ether na dogon lokaci. Gabaɗaya magana, yawan riƙe riƙewar ruwa na slurry yana ƙaruwa tare da karuwar abun ciki na Celullulose. Sakamakon riƙewar ruwa na sel mai ether hpmc na iya hana substrate daga cikin ruwa mai yawa da sauri, kuma tabbatar da cewa mahallin slurry yana samar da isasshen ruwa don ciminti hydration na ciminti. Bugu da kari, danko na Eler sel shima yana da babban tasiri akan ribar ruwa na turmi. Mafi girman danko, mafi kyawun riƙe ruwa. Gabaɗaya, etherulose ether hpmc tare da danko na 400ppta.s ana amfani dashi sosai a turmi na turmi da kuma ƙara matakin turmi da kuma ƙara ɗaukar nauyin turmi.

3. Komawa Lokaci: Elth eter yana da tasirin retard na turmi. Tare da karuwar abubuwan da ke cikin ether, saitin lokacin turɓaya na turmi. Tasirin Tasirin Cell Athulose HPMC akan ciminti Maste ya dogara da matsayin canjin kungiyar Alkyl, kuma yana da dangantaka da ƙwararrun dangantakar kwayar halitta. Karamin tsarin Alkyl, mafi girma cikin abun ciki na hydroxyl, kuma a bayyane yake sakamakon retarding. Kuma mafi girma abun ciki ether, mafi bayyane na jinkirta tasirin hadaddun fim a farkon hydration na ciminti, don haka tasirin retarding shima ya fi dacewa.

4. Karfin karfi da ƙarfin rikitarwa: yawanci, ƙarfi shine ɗayan mahimman mahimmancin kayan ciminti a kan cakuda. Versionarfin m da ƙarfi na turmi zai ragu tare da karuwar abun cikin HPMC abun ciki.

5. TARIHI: Cell Ather HPMC yana da babban tasiri a kan ɗaurin ragi na turmi. Cellulose ether fim fim tare da sakamako mai tasiri tsakanin ciminti na cikin tsarin polymer a waje da ciminti, wanda ke inganta bont na ciminti, don haka inganta bont na ciminti, don haka inganta bont ƙarfi na manna bayan hardening. A lokaci guda, madaidaicin da ya dace na etherulose yana haɓaka filastik da sassauci na turmi, yana rage ƙiyayya na yankin da ke tsakanin tursasawa da substrate na dubawa, kuma yana rage ikon zamawa tsakanin musayar. Zuwa wani lokaci, tasirin haɗin tsakanin turmi da substrate an inganta. Bugu da kari, saboda kasancewar Elet Elther a cikin ciminti na dubawa, wani yanki na musamman na Interface Layer an kafa tsakanin barbashi da samfurin hydration. Wannan Layer Layer sa yankin canja wurin dubawa mafi sassauƙa da sassauci, haka, saboda turmi yana da ƙarfin haɗin gwiwa.


Lokaci: Feb-27-2023